Detailed Environmental Impact Data

CO2 Emission Quantity

Unit: ton
/year 2010 2011 2012 2013 2014 2015

Sanjo Works

13,780 16,568 17,784 18,896 19,788 20,839

Technology Research Laboratory

1,418 1,847 1,635 1,534 1,466 1,336

Seta Works

2,537 3,708 4,166 4,454 5,195 5,283

Murasakino Works

375 491 491 481 413 373

Hadano Works

1,629 1,646 1,882 1,886 1,926 1,713

Atsugi Works

630 650 705 662 665 625

Shimane Shimadzu Corporation

2,673 2,254 2,574 2,650 2,420 2,156

Affiliated Companies in China

 4,561  4,828  4,757  5,135  4,872 4,359

Affiliated Companies in US

2,188 2,262 1,992 2,505 3,754 3,908

Affiliated Companies in Europe

1,232 1,302 1,685 1,811 1,912 1,580

Affiliated Companies in the Philippines

680 771 775 817 784 738

Note: The power conversion factor for each applicable year is calculated using the values published by the power companies under contact at each site, and the actual emission factors for each electric power supplier, published by the Japanese Ministry of the Environment.

Energy Usage

Unit: kL
/year 2010 2011 2012 2013 2014 2015

Sanjo Works

10,704 9,354 8,897 9,458 9,773  10,125
Technology Research Laboratory  1,150 1,052 818 768 723  647
Seta Works  2,091 2,061 2,076 2,225 2,557  2,556
Murasakino Works  282 275 246 241 205  181
Hadano Works  1,059 899 928 930 939  873

Atsugi Works

425 359 346 325 324  318
Shimane Shimadzu Corporation   968  895  925  953  891 812
Affiliated Companies in China   1,316  1,370  1,345  1,452  1,366  1,243
Affiliated Companies in US   1,039  761  1,143  1,141  1,858  2,005
Affiliated Companies in Europe   684  721  917  987  1,043 869

Affiliated Companies in the Philippines

 345  396  402  421  407  383

Note: All crude oil conversion values for power in the report are calculated with the coefficient for daytime power.

Waste Output

Unit: ton
 /year 2010 2011 2012 2013 2014 2015
Sanjo Works 1,770.7 1,579.8 1,616.4 1,675.1 1,788.5  1,855.3
Technology Research Laboratory  19.3 15.6 20.7 41.7 15.1  12.2
Seta Works  709.1 815.3 820.9 863.2 945.2  956.2
Murasakino Works  105.5 147.0 170.8 164.1 169.5  139.1
Hadano Works  128.2 146.4 143.6 103.3 108.0  167.1
Atsugi Works  13.6 13.5 14.8 11.1 12.4  20.7
Shimane Shimadzu Corporation 663.7 736.6 907.9

Note: The amount of waste discharged includes industrial waste, business related general waste, and valuables.

Recycling Ratio

unit:%
 /year 2010 2011 2012 2013 2014 2015
Sanjo Works  99.7 99.7 99.7 99.4 99.7  99.7
Technology Research Laboratory  79.4 73.1 81.2 95.1 79.8  71.0
Seta Works  100.0 100.0 100.0 100.0 100.0  100.0
Murasakino Works  98.9 98.4 99.5 99.5 99.4  99.4
Hadano Works  100.0 100.0 100.0 99.9 100.0  100.0
Atsugi Works  99.7 100.0 100.0 100.0 100.0  100.0
Shimane Shimadzu Corporation

99.0 99.1 99.3

※Recycling ratio = (Amount of waste discharged - Amount of final landfill disposal) / Amount of waste discharged

Tap Water Usage

Unit: m3
 /year 2010 2011 2012 2013 2014 2015

Sanjo Works

222,653 199,006 195,979 207,902 178,616 161,753

Technology Research Laboratory

11,756 10,037 10,415 9,578 8,281  7,581

Seta Works

10,519 9,806 10,918 12,244 12,596  15,563

Murasakino Works

3,999 4,818 5,379 4,943 3,712  3,761

Hadano Works

10,464 10,939 11,262 10,492 7,522  8,048

Atsugi Works

6,596 9,038 6,407 4,382 3,922  3,648

Shimane Shimadzu Corporation

3,299 3,269 3,494 3,576 3,331 3,477
Affiliated Companies in China
18,322 21,373 18,955 26,150 33,035  44,763
Affiliated Companies in US
 4,080  4,627  6,667  5,337  5,162  37,413

Affiliated Companies in Europe

4,294 3,206 3,204 2,674 3,387 2,930
Affiliated Companies in the Philippines
 8,767  11,765  12,569  12,569  16,420  15,029

Usage of PRTR-Reported Substances

Unit:kg

Reporting Business Organizations and Substances Used (Substance No.)

2010 2011 2012 2013 2014 2015

Sanjo Works

Acetonitrile(13) 1,016  
HCFC-225(185) 2,233 2,425  -
Toluene(300)   -  -  -  -  -  1,140
Nickel and their compounds(309) 4,019 3,538 2,987 3,579 4,409 4,655

Technology Research Laboratory

Selenium and their compounds(242) 1,060  

Seta Works

Xylene(80) 1,740 1,585 1,542 1,196  1,414 1,570
Toluene(300) 1,082  -

Note: The substance No. corresponds to the current PRTR method. Only substances reported to the administration are counted. A "-" in the table indicates less than 1 ton.

Unit:kg
  2010 2011 2012 2013 2014 2015

Sanjo Works

6,252 5,963 4,003 3,579 4,409 5,795

Seta Works

1,740 2,667 1,542 1,196 1,414  1,570

Technology Research Laboratory

0 1,060 0 0 0  0

Details on Content Reported for PRTR in 2015

単位:kg

Notification business office and substance to be used (substance number)

Amount of use

Emission to the atmosphere

Emissions to public water bodies

Emissions to soil at the establishment

Landfill treatment at the establishment

Move to sewer system

Move out of the establishment

Recycling

Emissions as products

Use

Sanjo Works

Toluene(300) 1,140 630 58 452

Painting, Washing

Nickel and its compounds(309) 4,655 2,000 2,655

Plating

Seta Works

Xylene
(80)
1,570 1,570 Painting