No.1pump : YP10 No.2pump : YP10 No.1pump : YP15 No.2pump : YP15
size 0.8-3.5 cc 0.8-7 cc 5-13 cc 5-16 cc
Rated pressure Max 20.6 MPa Max 20.6 MPa Max 20.6 MPa Max 20.6 MPa
Material of body Aluminum alloy Aluminum alloy Aluminum alloy Aluminum alloy

Open the table in a new window.

SD series

SD series
  SD1 series SD series
No.1pump : SGP1 No.2pump : SGP1 No.1pump : SGP2 No.2pump : SGP2
size 16-36 cc 16-36 cc 20-52 cc 20-52 cc
Rated pressure Max 20.6 MPa Max 20.6 MPa Max 24.5 MPa Max 24.5 MPa
Material of body Cast iron Cast iron Cast iron Cast iron

Open the table in a new window.

SDY series

SDY series
  SDY1 series SDY series
No.1pump : SGP1 No.2pump : YP15 No.1pump : SGP2 No.2pump : YP15
size 16-36 cc 5-16 cc 20-52 cc 5-16 cc
Rated pressure Max 20.6 MPa Max 20.6 MPa Max 24.5 MPa Max 20.6 MPa
Material of body Cast iron Aluminum alloy Cast iron Aluminum alloy

Open the table in a new window.

SD620 series

SD620 series
  SD620 series
No.1pump : SGP600 No.2pump : YP15
size 40-60 cc 5-9.5 cc
Rated pressure Max 25.0 MPa Max 13.7 MPa
Material of body Cast iron Aluminum alloy

Open the table in a new window.

DDG series

DDG series
  DDG05 series DDG1 series
No.1pump No.2pump No.1pump : SGP1 No.2pump : SGP1
size 4-16 cc 4-9.5 cc 16-27 cc 8-16 cc
Rated pressure Max 20.6 MPa Max 20.6 MPa Max 20.6 MPa Max 20.6 MPa
Material of body Cast iron Cast iron

Open the table in a new window.

DNP21S series

DNP21S series
  DNP21S series
No.1pump No.2pump
size 4.5-14cc 2.7-4.5cc
Rated pressure Max 20.6 MPa Max 20.6 MPa
Material of body Cast iron Aluminum alloy

Open the table in a new window.

This page may contain references to products that are not available in your country. Please contact us to check the availability of these products in your country.

TOP