Observation Examples of Metals
Observation of Copper Plate
![Observation of Copper Plate](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn5042000000726w-img/qn5042000000727d.jpg)
An electrochemical reaction has been caused in a copper plate in solution, and the surface form changes are observed in situ. This is the stage where cyclic voltammetry from - 600 mV to 800 mV has been repeated three times in a solution of 1 mM KCL, 5 mM CuCl2. (Using electrochemical solution cell and electrochemical controller)