Observation Examples of Nonmetals
Observation of Recycled Paper
![Observation of Recycled Paper](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000072m6-img/qn504200000072mn.jpg)
The topographic image (left) is unclear but the phase image (right) shows with good resolution the micro-structure of the fiber. (Using phase imaging system)
The topographic image (left) is unclear but the phase image (right) shows with good resolution the micro-structure of the fiber. (Using phase imaging system)