Observation Examples of Nanotechnology
Fullerene Nanowires
![Fullerene Nanowires](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000074ct-img/qn504200000074da.jpg)
Self assembled fullerene Nanowires. The stripe pattern at several nm intervals was observed.
(Courtesy of Dr. Takashi NAKANISHI, Supermolecules Group, Organic Nanomaterials Center, National Institute for Materials Science)