Observation Examples of Thin Film
Observation of Diamond film
![Observation of Diamond film](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/qn504200000075af-img/qn504200000075aw.jpg)
This is a diamond formation on a silicon Substrate. The diamond grows selectively following along the groove.
(Courtesy of Dr. Takaya, Department of Precision Engineering, Chiba institute of Technology)