0

    Microplastics Dynamic Particle Image Analysis System

    A dynamic particle image analysis system is suitable for analysis of the shape and particle count concentration (particles/mL) of microplastics dispersed in solutions. Although analysis of individual microplastic particles is also possible by stereomicroscope, the burden on the operator is large and analysis efficiency is poor. A dynamic particle image analysis system can automatically detect particles with sizes of 5 to 100 μm dispersed in a solution and analyze their shape and particle count concentration in a short time.
    Infrared microscope, which excels in analysis of organic compounds, is suitable for qualitative analysis of microplastics with sizes of 100 μm or less that can be captured with filter paper.

    Here, we introduce an example of analysis of the shape and particle count concentration of particles contained in environmental water and their qualitative analysis by using a dynamic particle image analysis system and an infrared microscope.

    Fig. 1 Particle Images

    Fig. 1 Particle Images

    Fig. 2 Histogram (Frequency Distribution Graph)

    Fig. 2 Histogram (Frequency Distribution Graph)

    From Fig. 1, the shapes of particles with sizes of 100 μm and less have be captured clearly, and various shapes, such as rod- like and fibrous shapes, can be confirmed.

    Fig. 3 Visual Observation Image

    Fig. 3 Visual Observation Image

    Fig. 4 Infrared Spectrum of Rod-like Microplastics

    Fig. 4 Infrared Spectrum of Rod-like Microplastics

    As a result of the qualitative analysis of the infrared spectrum (Fig. 4) of the area in the red circle in Fig. 3, this particle was identified as polypropylene (PP).

    By using the iSpect DIA-10 dynamic particle image analysis system, the shapes of the large number of particles contained in an environmental water sample could be observed efficiently, and statistical values for the size and shape and information on the particle count concentration could be obtained. The AIM-9000 infrared microscope enabled quick qualitative analysis of the composition of the microplastics captured by visual observation images, and its distribution could be shown clearly by using a chemical image.

    EDX

    Dynamic Particle Image Analysis System(iSpect DIA-10)

    This is a powder image analysis system in which images are taken of powders contained in a liquid test sample, and particle size analysis, shape analysis, and number concentration measurements are performed. When measuring liquid test samples that contain microplastics, particles are detected from the images taken, and information such as the number of such particles and their particle size distribution can be obtained in a short period of time.

    Read more

     
    AIMsight

    Infrared Microscope (AIM)

    Using an infrared microscope, microplastics collected on a filter paper can be identified and mapping analysis performed. Minute test samples can be measured with good sensitivity, and component analysis can be rapidly performed using an extensive library of standards.

    Read more

    English
    English (United States)
    Español (Estados Unidos)