    Dynamic Jack System - Specs

    Structural Fatigue Testing System (Jack System)

    Dynamic Jack System

    Load Method

    Electrohydraulic servo (capasity 10 to 300kN)

    Controlled Variables

    Load,displacement (strain)

    Test frequency

    0.001 to 30 Hz (The maximum varies depending on the hydrauli)