0

    EHV Series - Specs

    Servopulser Vibration Testing Machine

    EHV Series

    Vibration method

    Electro-hydraulic servo method

    Vibration force

    Horizontal 50 kN, vertical 40 kN

    Stroke

    ±50 mm

    Vibration direction

    Horizontal, vertical

    Control mode

    Peak values of displacement and acceleration