Language
Español
English
0

    SIE-560

    Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

    Measurement range

    Max. 560 mm

    Measurement principle

    High-precision magnetic induction linear sensor

    Measurement precision

    0.5 % or less or ±2.5 µm of indicated value, whichever is larger

    Gauge length

    10 mm to 550 mm

    Compliant Standards

    Plastics Tensile Testing Standard  ASTM D638
    Metallic Materials Tensile Testing Standards
    ISO 6892, JIS Z 2241, ASTM E8

    Applicable Specimens

    Steel, non-ferrous metals, composite materials (CFRP, GFRP, etc.), and general-purpose plastics

    Read more
    Show Less

    SIE-560S

    Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

    Measurement range

    Small range: Max. 4 mm
    Large range: Max. 560 mm

    Measurement principle

    Small range: Ultra-high precision strain gauge type sensor
    Large range: High-precision magnetic induction linear sensor

    Measurement precision

    0.5 % or less or ±1 µm of indicated value, whichever is larger

    Gauge length

    50 mm (can be optionally changed to 10 to 40 mm)

    Compliant Standards

    Plastics Tensile Testing Standard
    ISO 527, JIS K 7171, ASTM D638
    Metallic Materials Tensile Testing Standards
    ISO 6892, JIS Z 2241, ASTM E8

    Applicable Specimens

    Steel, non-ferrous metals, composite materials (CFRP, GFRP, etc.), and general-purpose plastics

    Read more
    Show Less

    SIE-560A

    Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

    Measurement range

    Max. (560 - gauge length) (mm)

    Measurement precision

    ± 1 µm, 0.5 % (JIS B7741 0.5 class)

    Gauge length

    10 to 550 mm

    SIE-560SA

    Automatic Extensometer SIE-560 [Standard Type] / 560S [High-Precision Type]

    Measurement range

    Max. (560 - gauge length) (mm)

    Measurement precision

    ± 1 µm, 0.5 % (JIS B7741 0.5 class)

    Gauge length

    50 mm (variable with option)

    Downloads

    Download the latest brochure.

    Do you live in the United States?

    Please visit our US website.