    Flexural Test Methods for Plastics: ISO 178 and JIS K 7171 - Specs

    Recommended Specimen

    ISO 178 and JIS K7171 Specimen and Fixture Dimensions

    Specimen length,l

    80 mm

    Specimen width,strong

    10 mm

    Specimen thickness,h

    4 mm

    Punch radius,R1

    5 mm

    Support radius,R2

    5 mm

    Distance between supports,L

    16h

    Read more
    Show Less

    3-Point Bend Test Fixture

    ISO 178 and JIS K7171 Specimen and Fixture Dimensions

    Specimen length,l

    -

    Specimen width,strong

    -

    Specimen thickness,h

    h> 3 mm

    Punch radius,R1

    5 mm

    Support radius,R2

    5 mm

    Distance between supports,L

    16h

    Read more
    Show Less

    3-Point Bend Test Fixture

    ISO 178 and JIS K7171 Specimen and Fixture Dimensions

    Specimen length,l

    -

    Specimen width,strong

    -

    Specimen thickness,h

    h≦ 3 mm

    Punch radius,R1

    5 mm

    Support radius,R2

    2 mm

    Distance between supports,L

    16h