    Sample Holder/Stocker for Contaminant Measurement

    EDXIR-Holder

    Suitable Instruments

    Shimadzu EDX Series, Shimadzu FTIR Series (with single reflection type ATR)

    Suitable Substances

    Resin piece, metal piece

    Part to Attach Samples

    Polypropylene film 25 μm thick and adhesive layer 10 μm thick

    EDX Beam Window

    Polypropylene film 5 μm thick

    Dimensions of Suitable Samples

    Max. 5 mm square, min. 1.5 mm square

    Thickness of Suitable Samples

    Recommended value when performing EDX measurement:
    Min. 0.5 mm, max. 1.5 mm (sample surface with no protrusions)
    Recommended value when performing FTIR measurement:
    Min. 0.1 mm, max. 4 mm (sample surface with no protrusions)

    Mass of Suitable Samples

    Max. 1 g