Observation of Copper Phthalocyanine

These images show copper-phthalocyanine crystals on a potassium-chloride substrate. It can be seen how copper phthalocyanine grows in the direction of the substrate’s crystal axis.
(Data provided by: Prof. Kobayashi, Institute for Chemical Research, Kyoto University)