Language
Español
English
0
Purified DWNT

Purified Double-walled carbon nanotubes(DWNT) were observed with Scanning Probe Microscope(SPM).
Observation of bundled and dispersed nanotubes is possible.
(Data provided by: Saito Laboratory, Graduate School of Engineering, Nagoya University)