This is an example of analyzing the organic solvents on the surface of photographic film. Samples were analyzed using headspace GC. 9-cm film samples were placed in vials, heated for 30 minutes at 90 °C, then 0.8 mL of their headspace was analyzed.
Example of GC Analysis