    Figs. 1 show the fishing nets and fishing lines collected at Majorca island in Spain and Texel island in the Netherlands. Figs. 2 show fishing nets obtained at a recycling plant. The results of measurement using FTIR showed that, polyethylene was the main component in many cases, and the other components were polypropylene .

     

    polyethylene, polypropylene

    Polyethylene,Polypropylene

    Results of Measurement Using FTIR of fishing Nets and Fishing Lines Collected on Beaches

    Figs. 1
    Results of Measurement Using FTIR of Fishing Nets Collected on Beaches

    Polyethylene, Polypropylene, Polyamides

    Polyethylene, Polypropylene, Polyamides

    Polyethylene, Polypropylene, Polyamides

    Figs. 2
    Results of Measurement Using FTIR of Fishing Nets obtained at a Recycling Plant

     
     
     
     

     
    FTIR

    Fourier Transform Infrared Spectrophotometer
    (FTIR)

    FTIR can qualitatively analyze organic matter and some inorganic matter, so it allows quick determination of the main components of fishing nets.