0

Showing

18
P/NProductSizeGuard ColumnGuard HolderUSP
227-31001-01 Shim-pack Bio IEX Q 30mmL.×4.6mmI.D., 5μm -
227-31001-02 Shim-pack Bio IEX Q 50mmL.×4.6mmI.D., 5μm -
227-31001-03 Shim-pack Bio IEX Q 100mmL.×4.6mmI.D., 5μm -
227-31002-01 Shim-pack Bio IEX Q-NP 30mmL.×4.6mmI.D., 3μm -
227-31002-02 Shim-pack Bio IEX Q-NP 50mmL.×4.6mmI.D., 3μm -
227-31002-03 Shim-pack Bio IEX Q-NP 100mmL.×4.6mmI.D., 3μm -
227-31003-01 Shim-pack Bio IEX Q-NP 30mmL.×4.6mmI.D., 5μm -
227-31003-02 Shim-pack Bio IEX Q-NP 50mmL.×4.6mmI.D., 5μm -
227-31003-03 Shim-pack Bio IEX Q-NP 100mmL.×4.6mmI.D., 5μm -
227-31004-01 Shim-pack Bio IEX SP 30mmL.×4.6mmI.D., 5μm -
227-31004-02 Shim-pack Bio IEX SP 50mmL.×4.6mmI.D., 5μm -
227-31004-03 Shim-pack Bio IEX SP 100mmL.×4.6mmI.D., 5μm -
227-31005-01 Shim-pack Bio IEX SP-NP 30mmL.×4.6mmI.D., 3μm -
227-31005-02 Shim-pack Bio IEX SP-NP 50mmL.×4.6mmI.D., 3μm -
227-31005-03 Shim-pack Bio IEX SP-NP 100mmL.×4.6mmI.D., 3μm -
227-31006-01 Shim-pack Bio IEX SP-NP 30mmL.×4.6mmI.D., 5μm -
227-31006-02 Shim-pack Bio IEX SP-NP 50mmL.×4.6mmI.D., 5μm -
227-31006-03 Shim-pack Bio IEX SP-NP 100mmL.×4.6mmI.D., 5μm -