SSG Series Strain Gauge Extensometers - Features
Elastic Modulus Measurements within 1 µm Accuracy - Compliant with Elastic Modulus Measurement Requirements of ISO 527, JIS K 7161, and Class B-2 for ASTM D638
Plastic tensile testing standards, represented by ISO 527, JIS K 7161, and ASTM D638, require high-accuracy displacement measurements.
The SSG series, widely used by plastics manufacturers, public testing institutions, and universities, meets the requirements of these plastic tensile testing standards.
ISO 527, JIS K 7161, and JIS K 7162 test standards require:
- Extensometer elongation measurements with accuracy within 1% of the measured value.
- Elastic modulus values based on a secant line or regression line between the two strain points of 0.0005 (0.05%) and 0.0025 (0.25%).
![](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/test/universal/qn5042000000kk0a-img/n9j25k00000pzv3g.jpg)
ISO 527, JIS K 7161, and JIS K 7162 Elastic Modulus Measurements
Satisfies Strain Control Requirements of ISO 6892 and JIS Z 2241
ISO 6892 and JIS Z 2241 detail test methods for determining the tensile strength of metallic materials. Included within these standards are two control methods for loading materials until they reach their yield point: a stress-rate controlled method and a constant strain-rate controlled method using an extensometer. ISO 6891-1 defines the strain rate control method as Method A, where testing using this strain rate control method is expected to become increasingly common.
![](/an/sites/shimadzu.com.an/files/d7/ckeditor/an/test/universal/qn5042000000kk0a-img/n9j25k00000pzv8n.jpg)
Shimadzu’s SSG series extensometers are ideal for strain-rate control testing according to ISO 6892 and JIS Z 2241.