0

    Autograph AGS-X Series - Specs

    AUTOGRAPH Table-TOP Precision Universal Tester

    AGS-10kNXD

    Specifications Table-top

    Max. Load Capacity

    10kN

    Crosshead
    Position
    Detection:Display Method

    Digital display (display resolution: 0.001 mm)

    Power Requirements

    Supply voltage fluctuations within ±10% of the set value.
    D-class (100 Ω max.) grounding resistance.

    Power Requirements

    Single phase 100/120/220/240 V AC
    (switching type) 50/60 Hz 1.2 kVA

    Weight

    85kg

    Dimensions

    W653×D520×
    H1603mm

    Accessories

    Load cell (with CAL cable), Power cable (2.5 m),turning rod, cable clamps, instruction manual

    Standard Functions

    • Analog recorder (option) output
    • Dataletty (option) output*5
    • Automatic test force / stress control (Autotuning)
    • Automatic strain control (Autotuning) *4
    • Test force auto-zeroing
    • Test force auto-calibration
    • Break detection, auto-return
    • Load cell overload detection
    • Touch-load detection function

    Standard Functions

    • External analog input (2 channels) *4
    • External digital input (2 channels) *4

    Standard Functions

    • Automatic reading of load cell characteristic values
    • Test force display, stress display, stroke display,position display
    • External analog output (2 channels)

    Sampling Speed

    1000Hz max. *4

    Crosshead
    Position
    Detection:Positional Accuracy

    ±0.1% indicated value or ±0.01 mm, whichever is larger

    Crosshead
    Position
    Detection:Measurement Method

    Optical encoder

    Lineup of Models Differing byLoad Cell Capacity

    1N /2N /5N /10N /20N /50N
    100N /500N
    1kN/ 5kN / 10kN

    Effective Test Width

    425mm

    Crosshead – Table
    Distance(Tensile stroke) *3

    1200mm
    (760mm, MWG)

    Crosshead Speed and
    Permitted Test Force

    To load cell capacity across entire speed range

    Crosshead Speed
    Accuracy*2

    ±0.1

    Crosshead : Max. Return Speed

    1500mm/min

    Crosshead : Speed Range

    0.001 to 1000 mm/min (stepless)

    Measurement : Calibration

    Automatic test force calibration: select tensile, compression, or
    tensile and compression

    Measurement : Accuracy : Standard-Precision Type (1/500, ±1%)

    Within ±1% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1,
    BS 1610 Class 1, and ASTM E4, JIS B7721 Class 1. *1

    Force:Accuracy : High-Precision Type
    (1/500, ±0.5%)

    Within ±0.5% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5,
    BS 1610 Class 0.5, and ASTM E4, JIS B7721 Class 0.5. *1

    Loading Method

    Direct high-precision constant speed strain control method via non-backlash ball-screw drive

    Operating Environment

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    AGS-50kNXD

    Specifications Table-top

    Max. Load Capacity

    50kN

    Crosshead
    Position
    Detection : Display Method

    Digital display (display resolution: 0.001 mm)

    Power Requirements

    Supply voltage fluctuations within ±10% of the set value.
    D-class (100 Ω max.) grounding resistance.

    Power Requirements

    Single phase AC200-230V 50/60Hz 4.0kVA

    Weight

    260kg

    Dimensions

    W718×D641×
    H1633mm

    Accessories

    Load Cell (with CAL cable), Power cable (5 m), turning rod, cable clamps, instruction manual

    Standard Functions

    • Analog recorder (option) output
    • Dataletty (option) output*5
    • Automatic test force / stress control (Autotuning)
    • Automatic strain control (Autotuning) *4
    • Test force auto-zeroing
    • Test force auto-calibration
    • Break detection, auto-return
    • Load cell overload detection
    • Touch-load detection function

    Standard Functions

    • External analog input (2 channels) *4
    • External digital input (2 channels) *4

    Standard Functions

    • Automatic reading of load cell characteristic values
    • Test force display, stress display, stroke display,position display
    • External analog output (2 channels)

    Sampling Speed

    1000Hz max. *4

    Crosshead
    Position
    Detection : Positional Accuracy

    ±0.1% indicated value or ±0.01 mm, whichever is larger

    Crosshead
    Position
    Detection : Measurement Method

    Optical encoder

    Lineup of Models Differing byLoad Cell Capacity

    50kN

    Effective Test Width

    425mm

    Crosshead – Table
    Distance(Tensile stroke) *3

    1210mm
    (745mm, MWG)

    Crosshead Speed and
    Permitted Test Force

    To load cell capacity across entire speed range

    Crosshead Speed
    Accuracy*2

    ±0.1

    Crosshead : Max. Return Speed

    1100mm/min

    Crosshead : Speed Range

    0.001 to 800 mm/min (stepless)

    Measurement : Calibration

    Automatic test force calibration: select tensile, compression, or
    tensile and compression

    Measurement : Accuracy : Standard-Precision Type (1/500, ±1%)

    Within ±1% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1,
    BS 1610 Class 1, and ASTM E4, JIS B7721 Class 1. *1

    Force : Accuracy : High-Precision Type
    (1/500, ±0.5%)

    Within ±0.5% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5,
    BS 1610 Class 0.5, and ASTM E4, JIS B7721 Class 0.5. *1

    Loading Method

    Direct, high-precision, constant-rate strain control using non-backlash precision ball-screw drive

    Operating Environment

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    AGS-100kNX

    Specifications Floor Type

    Capacity

    100kN

    Crosshead
    Position
    Detection : Display Method

    Digital display (display resolution: 0.001 mm)

    Dimensions

    W945×D725×H2164mm

    Accessories

    Load cell (with CAL cable), Power cable (5 m),turning rod, cable clamps, instruction manual

    Standard Functions

    • External digital input (2 channels) *4
    • Analog recorder (option) output
    • Dataletty (option) output *5
    • Automatic test force / stress control (Autotuning)
    • Automatic strain control (Autotuning) *4
    • Test force auto-zeroing
    • Test force auto-calibration
    • Break detection, auto-return
    • Load cell overload detection
    • Touch-load detection function

    Standard Functions

    • External analog input (2 channels) *4

    Standard Functions

    • Automatic reading of load cell characteristic values
    • Test force display, stress display, stroke display,position display
    • External analog output (2 channels)

    Test Method Files

    40 files (PC link: 20 files, standalone controller: 20 files)

    Sampling Speed

    1000Hz max. *4

    Crosshead
    Position
    Detection : Positional Accuracy

    ±0.1% indicated value or ±0.01 mm, whichever is larger

    Crosshead
    Position
    Detection : Measurement Method

    Optical encoder

    Loading Method

    Direct, high-precision, constant-rate strain control using non-backlash precision ball-screw drive

    Effective Test Width

    600mm

    Crosshead - Table Distance
    (Tensile stroke) *3

    1255mm (745mm, MWG)

    Crosshead Speed and Permitted Test Force

    To load cell capacity across entire speed range

    Crosshead Speed Accuracy *2

    ±0.1%

    Crosshead : Max. Return Speed

    1100mm/min

    Crosshead : Speed Range

    0.001 to 800 mm/min (stepless)

    Force
    Measurement
    : Calibration

    Automatic test force calibration: select tensile, compression, or tensile and compression

    Force
    Measurement
    : Accuracy : Standard-Precision Type(1/500, ±1%)

    Within ±1% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1, BS 1610 Class 1, and ASTM E4, JIS B7721 Class 1. *1

    Force
    Measurement
    : Accuracy : High-Precision Type(1/500, ±0.5%)

    Within ±0.5% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5, BS 1610 Class 0.5, and ASTM E4, JIS B7721 Class 0.5. *1

    Weight

    525kg

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    AGS-300kNX

    Specifications Floor Type

    Capacity

    300kN

    Crosshead
    Position
    Detection : Display Method

    Digital display (display resolution: 0.001 mm)

    Dimensions

    W945×D725×H2414mm

    Accessories

    Load cell (with CAL cable), Power cable (5 m),turning rod, cable clamps, instruction manual

    Standard Functions

    • External digital input (2 channels) *4
    • Analog recorder (option) output
    • Dataletty (option) output *5
    • Automatic test force / stress control (Autotuning)
    • Automatic strain control (Autotuning) *4
    • Test force auto-zeroing
    • Test force auto-calibration
    • Break detection, auto-return
    • Load cell overload detection
    • Touch-load detection function

    Standard Functions

    • External analog input (2 channels) *4

    Standard Functions

    • Automatic reading of load cell characteristic values
    • Test force display, stress display, stroke display,position display
    • External analog output (2 channels)

    Test Method Files

    40 files (PC link: 20 files, standalone controller: 20 files)

    Sampling Speed

    1000Hz max. *4

    Crosshead
    Position
    Detection : Positional Accuracy

    ±0.1% indicated value or ±0.01 mm, whichever is larger

    Crosshead
    Position
    Detection : Measurement Method

    Optical encoder

    Loading Method

    Direct, high-precision, constant-rate strain control using non-backlash precision ball-screw drive

    Effective Test Width

    600mm

    Crosshead - Table Distance
    (Tensile stroke) *3

    1475mm (635mm, MWG)

    Crosshead Speed and Permitted Test Force

    0.001 to 200kN:0.001 to 500mm/min(entire speed range) 200kN to 300kN:0.001 to 400mm/min

    Crosshead Speed Accuracy *2

    ±0.1%

    Crosshead : Max. Return Speed

    550mm/min

    Crosshead : Speed Range

    0.001 to 500 mm/min (stepless)

    Force
    Measurement
    : Calibration

    Automatic test force calibration: select tensile, compression, or tensile and compression

    Force
    Measurement
    : Accuracy : Standard-Precision Type(1/500, ±1%)

    Within ±1% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1, BS 1610 Class 1, and ASTM E4, JIS B7721 Class 1.*1

    Force
    Measurement
    : Accuracy : High-Precision Type(1/500, ±0.5%)

    Within ±0.5% indicated test force (at 1/250 to 1/1 load cell rating) 
    Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5, BS 1610 Class 0.5, and ASTM E4, JIS B7721 Class 0.5. *1

    Weight

    675kg

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    AGS-100kNX

    Specifications Floor Type

    Power Requirements : 400V model

    Three phases AC380-440V
    50/60Hz 4.5kVA
    Supply voltage fluctuations within ±10% of the set value.
    C-class (10 Ω max.)
    grounding resistance

    Operating Environment : 400V model

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    Power Requirements : 200V model

    A three phase AC200-230V
    50/60Hz 6.5kVA
    Supply voltage fluctuations within ±10% of the set value.
    D-class (100 Ω max.)
    grounding resistance.

    Operating Environment : 200V model

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    Power Requirements : 400V model

    Three phases
    AC380-440V
    50/60Hz 5.5kVA
    Supply voltage fluctuations within ±10% of the set value.
    C-class (10 Ω max.)
    grounding resistance.

    Operating Environment : 400V model

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    Power Requirements : 200V model

    A three phase
    AC200-230V
    50/60Hz 7.5kVA
    Supply voltage fluctuations within ±10% of the set value.
    D-class (100 Ω max.)
    grounding resistance.

    Operating Environment : 200V model

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    AUTOGRAPH Table-Top Precision Universal Tester

    Load capacity

    1 N to 10 kN (11 types)

    Test speed

    0.001 to 1,000 mm/min (Stepless)

    Test force accuracy

    Within ±0.5 % of display test force (for 1/1 to 1/500 of load cell capacity)

    AGS-X Series

    Load capacity

    1 N to 10 kN (11 types)

    Test speed

    0.001 to 1,000 mm/min (Stepless)

    Test force accuracy

    Within ±0.5 % of display test force (for 1/1 to 1/500 of load cell capacity)

    AGS-20kNXD

    Specifications Table-top

    Max. Load Capacity

    20kN

    Crosshead
    Position
    Detection:Display Method

    Digital display (display resolution: 0.001 mm)

    Power Requirements

    Supply voltage fluctuations within ±10% of the set value.
    D-class (100 Ω max.) grounding resistance.

    Power Requirements

    Single phase AC200-230V 50/60Hz 4.0kVA

    Weight

    235kg

    Dimensions

    W718×D641×
    H1633mm

    Accessories

    Load Cell (with CAL cable), Power cable (5 m),turning rod, cable clamps, instruction manual

    Standard Functions

    • Analog recorder (option) output
    • Dataletty (option) output*5
    • Automatic test force / stress control (Autotuning)
    • Automatic strain control (Autotuning) *4
    • Test force auto-zeroing
    • Test force auto-calibration
    • Break detection, auto-return
    • Load cell overload detection
    • Touch-load detection function

    Standard Functions

    • External analog input (2 channels) *4
    • External digital input (2 channels) *4

    Standard Functions

    • Automatic reading of load cell characteristic values
    • Test force display, stress display, stroke display,position display
    • External analog output (2 channels)

    Sampling Speed

    1000Hz max. *4

    Crosshead
    Position
    Detection:Positional Accuracy

    ±0.1% indicated value or ±0.01 mm, whichever is larger

    Crosshead
    Position
    Detection:Measurement Method

    Optical encoder

    Lineup of Models Differing byLoad Cell Capacity

    20kN

    Effective Test Width

    425mm

    Crosshead – Table
    Distance(Tensile stroke) *3

    1250mm
    (765mm, MWG)

    Crosshead Speed and
    Permitted Test Force

    To load cell capacity across entire speed range

    Crosshead Speed
    Accuracy*2

    ±0.1

    Crosshead : Max. Return Speed

    2200mm/min

    Crosshead : Speed Range

    0.001 to 1600 mm/min (stepless)

    Measurement : Calibration

    Automatic test force calibration: select tensile, compression, or
    tensile and compression

    Measurement : Accuracy:Standard-Precision Type (1/500, ±1%)

    Within ±1% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 1, ISO 7500-1 Class 1,
    BS 1610 Class 1, and ASTM E4, JIS B7721 Class 1. *1

    Force:Accuracy : High-Precision Type
    (1/500, ±0.5%)

    Within ±0.5% indicated test force (at 1/500 to 1/1 load cell rating)
    Conforms to EN 10002-2 Grade 0.5, ISO 7500-1 Class 0.5,
    BS 1610 Class 0.5, and ASTM E4, JIS B7721 Class 0.5. *1

    Loading Method

    Direct high-precision constant speed strain control method via non-backlash ball-screw drive

    Operating Environment

    Temperature: 5 °C to 40 °C; Humidity: 20% to 80% (no condensation)
    Floor vibrations: frequency 10 Hz max., amplitude 5 μm max.

    *1 Official certification after installation is recommended to comply with EN 10002-2, ISO 7500-1, and ASTM E4 standards, JIS B7721.
    *2 Crosshead speed accuracy is calculated from the crosshead travel within a prescribed time at a constant speed between 0.5 mm/minute and 500 mm/minute.
    *3 The tensile stroke is the effective stroke when SCG (screw-type flat grips) or MWG (non-shift wedge-type grips) are mounted.
    *4 TRAPEZIUM X or TRAPEZIUM LITE X is needed for these functions. Moreover, when automatic test force/stress control (auto tuning) and the automatic strain control (auto tuning) are used, the sampling speed becomes 10msec.
    *5 Dataletty (option) and TRAPEZIUM X / TRAPEZIUM LITE X can not be used together.
    * Values stated in this catalog are based on measurements conducted according to separately defined inspection standards.
    * Windows7/ Windows Vista/ Windows XP is a registered trademark in the United States and other countries of Microsoft Corporation

    Read more
    Show Less

    Do you live in the United States?

    Please visit our US website.