Shimadzu Review Vol.78[1・2](2021)
Industrial Machinery

SPECIALLY COLLECTED PAPERS

Development of a Compact Debinding and Sintering Furnace (VHS-CUBETM)
for Metal 3D Printing

by Yosuke Morimoto1

Shimadzu Review 78[1・2] (2021)

Abstract

Additive manufacturing is used in many markets and the size of the additive manufacturing market is set for growth. Shimadzu Industrial Systems Co., Ltd. has developed a compact furnace called VHS-CUBE suitable for debinding and sintering parts made by metal 3D printers.


1Research & Development Department, Industrial Machinery Division, Shimadzu Corporation, Kyoto, Japan

*The information contained in Shimadzu Review has not been modified since the original publication date. Please be aware that in some cases, products mentioned within the articles are no longer available.