0

UV-2600i Plus/UV-2700i Plus - Applications

NEW

UV-Vis Spectrophotometer

Electricity, Electronics, and Optics

Band Gap Measurements for Compound Semiconductors

Band Gap Measurements for Compound Semiconductors

The diffuse reflection spectra for two types of compound semiconductors (red line: Culn0.5Ga0.5Se2, blue line: CulnSe2) used as solar cell materials were measured using the ISR-2600Plus integrating sphere. It is evident that the absorption edge (position where the reflectance drops) differs depending on the sample. This difference signifies a difference in the band gap* for these samples. (The samples were provided by Wada Laboratory, Faculty of Science and Technology, Ryukoku University.) The band gaps for the samples were calculated utilizing the Tauc method. The results obtained were 1.27 eV for Culn0.5Ga0.5Se2 (red line) and 0.99 eV for CulnSe2 (blue line). * The term band gap refers to the energy difference between the top of the valence band, which is full of electrons, and the bottom of the conduction band, which does not contain electrons.

Chemicals

Thickness Measurements of Cling Films

Thickness Measurements of Cling Films

Undulating interference waveforms sometimes occur if light is passed through a film. The film thickness of a sample can be determined by using these interference waveforms. The figure shows transmittance data for a cling film. A clear interference waveform is produced. Utilizing optional film thickness measurement software, the film thickness is calculated as 10.4 μm. (Caution) The sample's refractive index must be entered for the film thickness calculation.

Medicines

Evaluating Thermal Stability (Tm) Analysis of Oligonucleotide Therapeutics

Evaluating Thermal Stability (Tm) Analysis of Oligonucleotide Therapeutics

Oligonucleotide therapeutics samples (9 to 60 M) were analyzed using TMSPC™-8i and 1 mm optical path length cells. Since UV-2600i Plus /2700i Plus can measure over a wide dynamic range, it is possible to perform a thermal stability analysis of nucleic acid drugs by obtaining the Tm value from the melting curve.

Construction

Window Glass Transmission Measurements

Window Glass Transmission Measurements

Two types of window glass were measured utilizing the ISR-2600Plus integrating sphere. The sample shown by the red line is highly transparent to near-infrared light at 800 nm or more. The sample shown by the blue line, however, is apparently not very transparent to near-infrared light.

Cosmetics

Measurement of the Ultra Violet Protection Factor Assigned to Ultraviolet Protection Clothes

Measurement of the Ultra Violet Protection Factor Assigned to Ultraviolet Protection Clothes

The UV protection provided by clothes and an umbrella were analyzed by an ISR-2600Plus integrating sphere accessory. The transmittance spectrum of the umbrella (green) shows that very little UV radiation transmits through the umbrella. In regards to the clothing, the black areas block more UV radiation than do the white areas.

Textiles

Total Transmittance Spectrum of CNF

Total Transmittance Spectrum of CNF

An ISR-2600Plus integrating sphere was used to measure the total transmittance spectrum of cellulose nanofiber (CNF). Depending on the raw materials used, spectra can vary, transparency can vary, and spectral tendencies in the ultraviolet region can vary.

Life Sciences

DNA and Protein Measurements

DNA and Protein Measurements

The red and blue lines are the absorption spectra for dsDNA and BSA (bovine serum albumin), respectively.
The concentration values are 45 ng/μL for dsDNA and 2.2 mg/mL for BSA.

Foods

Vitamin Measurements

Vitamin Measurements

This shows the absorption spectra for riboflavin (vitamin B2).
The sample concentrations are, in order from the highest absorbance, 0.08,
0.04, 0.02, and 0.01 mg/mL.