VHS Horizontal Vacuum Dewaxing-Sintering Furnace

VHS Horizontal Vacuum Dewaxing-Sintering Furnace

Features

  1. Performs Degassing, Dewaxing and Sintering in Sequence
    Uses internal tight box to discharge binder vapors and prevent them from adhering to or contaminating furnace walls or the heat-insulating layer.
  2. Used Extensively for Wide Variety of Applications and Purposes
    Furnace can be used for a wide variety of treatments and purposes, from low temperature heat-treatment, to high-temperature firing processing of ceramics and similar materials.

Applications

  • Superhard Alloys
    Performs dewaxing, degassing, and sintering in sequence
  • Non-Oxide Ceramics
    Performs dewaxing, degassing, and firing processes in sequence
    Application: Aluminum Nitride (AlN)
  • Metals
    Performs dewaxing, degassing, and sintering in sequence
  • Graphite
    Performs degassing and purification in sequence

PHS Series Specifications

     
Vacuum Sintering Furnace
Model VHSg
r20/20/50
VHSgr
30/30/60
VHSgr
40/40/100
VHSgr
50/50/120
Effective Intern. Dim. (mm)
W x H x D
200x200x500 300×300×600 400×400×1000 500×500×1200
Max. Temp. (°C) 1600
〈2400〉
Process. Cap. (kg gross) 50 100 250 400
Ultimate Press. (Pa) 7×10-1
(7×10-3)
Max. Pressure Atmospheric Pressure
Power Req. (kVA) 70 90 140 170
Gases N2,Ar,(H2)